    Another Common question – How can we extend the Primer recoat window if we have to –

    The max recoat window of Civilox LV100 that is not exposed to UV at 25 deg C is 3 days. The max recoat window of Civilox LV100 that is not exposed to UV at 15 deg C is 6 days.
    If your average temperatures are below 25 deg C your recoat window will be longer than 3 days.
    The Cvilox LV100 is a sealer that is designed to have low viscosity for concrete penetration. Repeat application of Civilox LV100 will make a very smooth surface that will reduce adhesion.
    Concrete will sometimes require two applications of Civilox LV100 for sealing purposes. For further applications to extend the recoat window I recommend the Civilox HB200, its higher PVC formulation will improve adhesion. If the Civilox LV100 is outside its recoat window then surface preparation will be required.